But isn't this just ordinary work hardeneing of the material?
Charles
Scott Lane wrote:
>
>> Wouldn't heating it to critical temp undo any compaction? I
>> understand in as left the mill state the surface is compacted ( belt
>> sand off one side of a cold rolled flat bar and let it sit for a
>> while to see the effects) , but does the effect survive the forge?
>
>
> I don't think just heating it to critical temp will undo
> physical movement of the material. It's not compacted through the
> entire piece, just the surface. Think of a plain M&M; hard shell with
> softer inside...
>