Hey Guys,

Probably a very pedestrian question for most of you metal manglers out there, but I have never had the need or motivation to forge a flour-de-lis from a piece of plat stock before, and I have a client who wants that kind of detailing.

I know it involves hot cutting into the flat and bending the sides into curves, but I am looking to make it elegant versus what I envision for a process.

Ray Miller