Any Low Carbon stainless rod "L" designation.
the good ol' 7024 rod has great penetration, but use a nickel or
stainless rod for good adherence to the iron.
Ray
On Saturday, November 22, 2003, at 05:17 PM, Barking Crow wrote:
> Hey Ray,
>
> Does it matterwhich stainless rod?
>
> I've been working on an old Prentiss bench vise that I've never seen
> one of
> before. Instead of a large square shaft on the moveable jaw that
> surrounds
> the screw it has two guides, both about 3/4 and 1 3/4. One is abouve
> the
> screw and parralel to the ground and one below the screw and
> perpendicular
> to the ground. Seems like a nice design. The moveable jaw was broken
> clean
> at the top of the upper guide. I deeply grooved it all around on both
> pieces and then filled in the grooves. I didn't try it, but was
> wondering
> if I could have done the outer welding that was really just to rebuild
> the
> curvature of the upper jaw with my favorite 7024 rod. Would it have
> damaged
> the lower repair that was with the nickel rod?
>
> Thanks again for all your advice.
>
> Jeff Valentine
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>