Just make sure that you get stainless welding rod with the "L" <for "low carbon"> designation. This is IMPORTANT. Then follow all procedures like you would for the nickle rod. Dave Brown 1/22/03, you wrote: >Hey Jeff!! > >It's not advertised often but in many cases you can actually use stainless >rod for cast iron. Preheat and cool slowly. >Ray >Cincinnati