Hey Jeff!!

It's not advertised often but in many cases you can actually use 
stainless rod for cast iron. Preheat and cool slowly.
Ray
Cincinnati

On Saturday, November 22, 2003, at 12:26 PM, Barking Crow wrote:

> Home Depot and Lowes have stopped carrying the 55% and 99% Nickle 
> welding
> rods for welding cast iron.  Can someone recommend a good place to buy 
> small
> boxes of them online?
>
> Thanks,  Jeff in Tallahassee
>
>