PROCESS
Axial - Wire Dia. .030 Amps 115-200 Volts 15-27 Gas 75% Ar+ 25%CO2
Spray - Wire Dia. .035 Amps 165-300 Volts 18-32 Gas 98%AR + 2% 02
Spray - Wire Dia. .045 Amps 200-450 Volts 20-34 Gas 98%AR + 2% 02
I have never been able to get non html formated stuff to line up either.
Darrell
http://www.machinemaster.com
----- Original Message -----
From: "Kenny O." <[email protected]>
To: <[email protected]>
Sent: Friday, November 21, 2003 3:47 PM
Subject: [TheForge] spray Arc
> Let me try this again .
> I cant seem to make this typing thing get there
> the same way it looks when I start.
>
>
>
> process | WIRE DIA. | AMP RANGE | VOLT RANGE
> | shielding gas
> --------------------------------------------------------------------------
-----------------------------------------------
> axial .030 115 -
> 200 15 - 27 75% Ar+ 25%CO2
> spray .035 165 -
> 300 18 - 32 or
> 045 200 -
> 450 20 - 34 98%AR + 2% 02
>
> I hope it works this time
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>