the same way it looks when I start.
process | WIRE DIA. | AMP RANGE | VOLT RANGE
| shielding gas
-------------------------------------------------------------------------------------------------------------------------
axial .030 115 -
200 15 - 27 75% Ar+ 25%CO2
spray .035 165 -
300 18 - 32 or
045 200 -
450 20 - 34 98%AR + 2% 02