In addition to Ralph's question, how tight to the cast does it have to be?
I'd imagine minimal gaps? Kevin
-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Ralph Sproul
Sent: Tuesday, 04 November, 2003 4:54 PM
To: [email protected]
Subject: Re: [TheForge] Re: Burning Metal
Hi Pete, That's an interesting idea - I've never tried that, but would like
to. Do you use something light like 1/4" or does it take 1/2 to keep the
oxidizing stream going?
Ralph
----- Original Message -----
From: "Peter Fels And Phoebe Palmer" <[email protected]>
To: <[email protected]>
Sent: Monday, November 03, 2003 9:13 PM
Subject: Re: [TheForge] Re: Burning Metal
> One can use a sacrifice piece of steel to sustain a torch cut in cast
> iron..carbon isn't the critical factor..plain iron seems to be...PF
>
> Andy Gladish wrote:
>
> >>I think if the carbon content was the accelerating factor, cast
> >>iron should
> >>cut easily.
> >>The best I can do on cast iron with an O/A torch is a very sloppy cut.
> >>My plasma torch however cuts it easily.
> >>chuck-
> >>
> >>
> >
> >I think that what is happening when I use an O/A torch to cut cast iron
is
> >that the preheat is melting the metal and the oxygen jet is blowing it
> >aside. Way different from the sharp, clean cut (burn) I get with steel
when
> >things are set up correctly.
> >So, a torch will 'cut' things that it can't 'burn'.
> >Andy G.
> >
> >_______________________________________________
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login: [email protected]
> >password: anvil
> >___________
> >
> >
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________