Norm, all I'll add is that castable can set pretty quickly. You might
try a handful and see how quick.
Steve Smith
[email protected] wrote:
> I know this has been discussed before on theforge but I didn't pay
> enough attention. I have an atmospheric forge that works well and is
> lined with 2" of kaowool and then covered with ITC 100.
>
> Now I want to make a forge that is lined with Mizzou castable
> refractory 3000 degree.Just got the refractory today (55 lbs for
> $27.50) but no info with it or on the bag as far as specifications or
> applications are concerned. I assume I just mix water with it and not
> make it too soupy--I'll just wait plenty long for it to set up. What I'm
> wondering is:
>
> Does it help to put a short metal rods, screws, or whatever through
> the sides of the forge to help hold the lining in place once dry?
> What's the best thing to use?
>
> What's the best way to make a removable form to fit the inside of the
> forge to shape the inside opening?
>
> What are the disadvantages and advantages of using castable
> refractory as opposed to kaowool or durablanket type insulation?
>
> Does Mizzou type material make a good floor for a forge?
>
> I plan to make the forge out of about a 10" or 12" pipe with about a
> ..09 wall and form a flat place in the pipe for the bottom of the forge.
>
> Been thinking about making the thickness of the insulation
> somewhere between 1.5 and 2 inches. Will this be adequate?
>
> Any suggestions or tips anyone has will be truly appreciated.
> Thanks in advance for your help.
>
> Norm Larson
>
>
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>