I receive the following post from the Guild of Metalsmiths and thought it
would be appropriate to pass it on to theforge, especially since the
subject of die steels came up.
>4340 is basically the same as 4140 with the addition of 1.5/2.0 % Nickel
>and is usually considered to have slightly better fatigue properties. It
>is more susceptible to quench cracking (Should not be water quenched) and
>should be tempered back immediately after quenching.
>
>thanks,
>Dave Tokle
>Metallurgical/Quality Engineer
>SPX Service Solutions