Ok, they show that each tooth is alternatingly offset which is no big 
deal.  But, I had 2 ideas for cutting the teeth.  1) Triangle file  2) hot 
cutting.  What I don't know is the profile of the tooth itself.  This is a 
little hard to explain but did you put a cutting edge on the tooth other 
than the peak of each tooth?

Dan

At 11:09 PM 3/19/2003, you wrote:
>Dan:
>
>I did the hacksaw.  All wrought iron.  I made a test blade with  case
>hardened teeth that cut the parent metal.  Didn't choose to harden the
>blade on the display piece.
>
>Give a holler with your questions.
>
>Ken Zastrow