Larry,

Item 22 is actually listed as a bucket handle.  I'm including the text
for the bucket mount and the handle, just in case you want to make the
whole bucket, hint, hint, hint.  Here's the text:

Index:

21-22		(?)bucket mount and handle	pls. 10 and 24-25
p. 11

page 11:

(?)Bucket mount of iron						Pl.
25:21

Three pieces of wide iron band, one edge of which is turned over.  This
was probably the rim mount of a (?)wooden bucket, with the remains of a
riveted handle attachment.  The longest piece is made up of two sheets
joined together by a vertical row of rivets.  A roughly rectangular
mount, which clearly ends in a damaged loop just above the turned edge,
is attached by rivets to the joined bands.
  A rivet-hole about 4 cm from the upper edge of the other portion of
the band suggests the position of the second handle attachment; there
are also traces of rust here.  At the lower edge of the band at least
one rivet-hole can be distinguished.
Band, width 9.9 cm, total length about 113 cm (70 + 23 + 20cm);
thickness of plate about 0.2cm.

Handle of Iron							Pls. 10
and 24:22

Iron handle, possibly associated with the mount no. 21 (see above). It
is made from a broad, flat iron rod with an open hook at each end.
Before conservation one of the hooks retained a fragment of the loop to
which the handle had been attached.  This loop seemed to be of the same
dimensions and appearance as the loop which is attached to the iron
mount no. 21.  The distance between the hooks (outside measurement)is 38
cm, but the curvature of the handle has been exaggerated by bending.  
Width 2.3 cm, thickness 0.20-0.35 cm, length 38 cm, height 18.6 cm.


Bill Clemens



-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Larry Brown
Sent: Tuesday, March 11, 2003 8:01 PM
To: [email protected]
Subject: RE: [TheForge] Mastermyr II

Hi
To anyone with the Mastermyr book, I can't seem to find a description
for 
item #22 (cauldron handle) on the web site, is it in the book?
Thanks
L Brown

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________