We use antifreeze! Glycol fills pores/cells, and does'nt seem to dry out as
quickly.
Plus , nice finish on steel.



dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message ----- 
From: "klgeorge" <[email protected]>
To: <[email protected]>
Sent: Friday, June 27, 2003 4:06 PM
Subject: [TheForge] hammer handles


> let them dry out then soak in soapy water. This may take a few times to
> fill the pores. For new handles ,fit handle remove and coat the eye with
epoxy.
>