For Incralac, a West-coat supplier is Conservator's Emporium, Inc 100
Standing Rock Circle, Reno NV. (775) 852-0404. This product is intended
for non-ferrous metals, esp.copper and bronze. I have not been able to find
a similar specific product for ferrous metals.
Grant
----- Original Message -----
From: "Fiorini & Skiles" <[email protected]>
To: <[email protected]>
Sent: Thursday, June 05, 2003 5:20 AM
Subject: [TheForge] incralac supplier in USA
> Custom Aerosol Packaging
> PO Box 1411
> Piqua, OH 45356
> 937-773-1824
>
> Forgive me if this is a repeat. I looked it up in the shop yesterday.
You
> can get a small quantity, which they call their "touch up" can. You can
> also get an aerosol spray can.
> This stuff has 3 very toxic solvents in it- xylol, acetone and something
> else that I can't remember.
> -Kirsten
> [email protected]
> http://home.centurytel.net/Fiorini_and_Skiles
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>