[TheForge] In a pickle now!

Steve Bloom [email protected]
Mon Jul 21 12:57:01 2003


At 08:23 AM 7/21/2003 -0700, you wrote:
>Well, the cannon project has run into a snag.

(description of jammed sleeve snipped)
In any event, I'm in a pickle now with the sleeve 6"
>into the bronze 'n' tight as he!!

Hokay -- plan B -- cut off the steel sleeve at the end of the bronze. Use a 
hacksaw/ grinder/whatever and slit the steel -- taking real care not to cut 
into the bronze.
roll the sleeve the steel into a smaller tube and remove -- this is the 
usual formula for removing a rusted bushing sleeve in the suspension of a 
240Z. -- replace the
steel and redimension the clearance. Try again.  Not pretty but better than 
junking both.