I run them at about 180 a. AC
dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message -----
From: "Alix Peshette" <[email protected]>
To: <[email protected]>
Sent: Sunday, July 20, 2003 12:20 PM
Subject: RE: [TheForge] Anvil Refacing
> Hi Dan,
> Thanks for the info about the MG750 rod. Can it be used with a 225 amp AC
> buzz box?
>
> -Alix
> Voodoo Moon Forge
>
> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On Behalf Of Dan Tull
> Sent: Sunday, July 20, 2003 6:29 AM
> To: [email protected]
> Subject: [TheForge] Anvil Refacing
>
>
> I sure wish some of you would try some refinishing w/ the rods we have
been
> using for about 10 years.
> We have had excellent luck, no call backs, not chipping, and it makes it
so
> easy, everyone can start
> refacing anvils. You can tie top to base w/ 6010/6011 as underlayment.
>
> MG750 rod. from MG Industries, for the rock crushing industry, "highest
> impact"resistance
>
> Pros:
> Used to join dis-similar steels( tool to mild)
> NO PREHEAT
> Hammer to stress relieve
> Work hardens
> Can be re- coated w/ Mg760 for addtional hardness
>
> Cons:
> Cost- $2.20 each rod
> Availibility- I have two local dealers that carry them ( Holox )
> Color match- high manganeze so it rusts out silver
>
> More later.
> dan tull
> georgia
> abba, afc, S.C. psba, obg,sofa
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>
>