[TheForge] Portable Forge rebuild
Roy Wilson
[email protected]
Wed Jul 16 11:45:07 2003
On Wed, 16 Jul 2003 10:06:52 -0500, Best, Dianne wrote:
>#2 - Broken drive wheel
>A segment (between two spokes) fell out of the large flywheel that drives
>the blower. The ends are rusty, so it has been broken for a long time.
>I know how cast iron is SUPPOSED to be brazed (by evenly preheating,
>brazing, and the slowly and evenly allowing to cool) but I haven't had much
>luck with that process - I have had new cracks form during cooling.
>I am thinking about repairing the flywheel segment by using epoxy and
>putting in a couple of small steel pins. Is there an easier way?
Electric weld it using a pure nickel rod. I think there
are some other rods available for use on cast iron and cast steel
as well.
Roy Wilson
General Operations Director
Zanzibar Internet Land Line Administrator
<[email protected]>