Thats part of the problem...

I've moved the compressor to another building so I can hear myself think 
between heats...

Outa site outa mind...so they say...

mike

At 10:57 PM 7/4/2003 -0500, you wrote:
>I do no trust my automatic vent to keep the tank dry. Try running a 1/8
>inch copper tube from the manual drain port to a ball cock placed where
>you see it when you go for the light switch. Blowing it off manually
>once or twice a day
>should keep the tank dry.
>
>Even with the automatic drain working there still seems to be plenty in
>the line when I drain it,
>
>Mike Graf.


            Mike Linn
      Artist Blacksmith
          McCalla, AL
        AFC Webmaster
http://afc.abana-chapter.net