[TheForge] Welding a whole lotta cast iron
Mike Sweany
[email protected]
Tue Jul 1 14:30:00 2003
you might include a couple weed burners to keep the frame at temp while welding on it.
prolly 600f. or so gonna be a tough job. Hope this is just a show tractor. Maybe a few hidden bolted "patch plates" if there is room. Good Luck and pass the GATORE AID.
irontree <[email protected]> wrote:
Hi all,
In effort to keep my neighbors happy, I do small welding jobs for
free. ...well....A neighbor brought me his antique tractor (big!!!). The
entire front frame is cracked down from the top of the tractor down through
to where it connects to the front wheels. He wants to weld it back
together. (about 4ft high and 18 inches wide)
My thoughts...
1. Jack up the front and remove the front frame from tractor.
2. Grind a nice clearance so I get good penetration.
3. Build a big bonfire and toss the frame in and heat it up.
4. Pull it out and weld with nickel rod or other recommended rod
5. toss it back the fire to equalize the heat
6. finish weld
7. toss it back the fire to equalize the heat and leave in fire until it
goes out.
8. pull out in the morning and reattach.
suggestions? This is a bigger weld job than I have ever done. I already
told him that I wouldn't guarantee it.
dan
www.irontreeworks.com
-----Original Message-----
From: Marc V. Davis III (Marc of the Hammer)
To: [email protected]
Date: Monday, June 30, 2003 11:53 PM
Subject: [TheForge] patinas or chemicals for Steel in Michigan
>I know this has probably been asked before but does anyone know if there is
>anyplace to get patinas or chemicals for Steel in Michigan?
>Thanks
>Marc
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________
>
>
>
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________
---------------------------------
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed. To learn how
to post in Plain-Text go to: http://www.expita.com/nomime.html ---