This is one thought I had.  Again the object is to overcome the mass of
the ram, with as small amount of energy required to get it moving.

Marc Godbout wrote:

> Here's another thought. If the counterweight is just like a see-
> saw, on the straight arm of the driving head, it would end up in
> the "top" position when the hammer hits the work. How about
> arranging it so that the counterweight arm is short, and parallel
> to the floor when the hammer is hitting. Then you'd get the most
> benefit from gravity on the return. And it would "weigh" less when
> starting the stroke.
>

I have also looked at the spare flywheel from a LG sitting on the
ground.  But then as George said, do I really want a treadle powered LG?

Larry

>
> As Pete said, there is still some loss in the transmission, no
> matter how the masses are arranged. A shorter counterweight arm
> take some flex out of the system. Now I'm thinking some wheel
> instead of an arm.
>
> Someday I may actually build one of these instead of think about
> it :-)
>
> -Marc
>
> ---------- Original Message ----------------------------------
> From: Peter Fels and Phoebe Palmer <[email protected]>
> Reply-To: [email protected]
> Date:  Fri, 24 Jan 2003 01:27:50 -0800
>
> >At 12:27 PM 1/23/03, you wrote:
> >
> >
> >I was wrong when i said that a split weight ( counterbalancing )
> would be
> >slower..misread, sorry.
> >But if the hammer head only had 1/2 the weight  it would be less
> efficient
> >because the mechanism would absorb some of the blow. Think of how
> much
> >difference there is  just working on the heel VS the middle of
> the anvil
> >face.  When the hammer isn't directly above the work and/or the
> anvil mass
> >isn't directly below the work, considerable loss is the result.
> To get the
> >same forging effect, the counterbalanced assembly would have to
> be
> >considerably heavier than a conventional sprung TH. It would,
> however, have
> >some compensating virtues. If nothing else, those tensioned
> springs spook
> >me. Garage door springs kill people.
> >Larry, why bother with a light spring? just shift the
> counterweight out a
> >little.....Pete
> >
> >
> >
> >
> >>Like a teeter toter?
> >>Saw one of those in a website with some Asian content. Two kids
> stood on
> >>the back. Rails on the side of the beam so they. When a hit was
> callled
> >>for they just pushed down on the beam. Yeah could work if yoou
> have smart
> >>weights.
> >>  DragonsWatch <[email protected]> wrote:I have looked
> at the
> >> designs of several different styles of treadle hammer. And they
> all seem
> >> to have one thing in common, some sort of lever and large
> springs which
> >> lift the hammer, and a treadle to over come the springs and
> lower the
> >> hammer. So I ask, what would be the result if the springs were
> replaced
> >> with a weight great enough to balance the hammer. Then a light
> spring
> >> could lift the hammer. Say a conventional design has a hammer
> of 50# and
> >> the operator can accelerate that weight to say 5 fps and the
> travel is 8
> >> inches. You would have an
> >>impact of XXX pounds per sq. inch. If you had a hammer where the
> head was
> >>balanced, say 25# hammer and 25# counterweight, would it not
> strike at the
> >>same pounds per sq. inch when moving at 5 fps?
> >>This does require the ram and the weight be rigid to each other.
> The point
> >>being is that you still have 50# of mass in motion, and the
> energy is
> >>transferred in the blow, not in the motion of the head. Seems
> somewhere it
> >>is written that a mass in motion will remain in motion, or
> something like
> >>that. Just something to think about. I'm sure I am over looking
> some
> >>obvious law of physics that says this is not how things work.
> >>
> >>Larry
> >>
> >>
> >>_______________________________________________
> >>http://mailman.qth.net/mailman/listinfo/theforge
> >>theforge mail list group photo site is
> >>http://www.photoaccess.com
> >>Login: [email protected]
> >>password: anvil
> >>___________
> >>
> >>
> >>
> >>
> >>---------------------------------
> >>Do you Yahoo!?
> >>Yahoo! Mail Plus - Powerful. Affordable. Sign up now
> >>
> >>--- StripMime Report -- processed MIME parts ---
> >>multipart/alternative
> >>   text/plain (text body -- kept)
> >>   text/html
> >>The reason this message is shown is because the post was in HTML
> >>or had an attachment.  Attachments are not allowed.  To learn how
> >>to post in Plain-Text go to: http://www.expita.com/nomime.html  -
> --
> >>_______________________________________________
> >>http://mailman.qth.net/mailman/listinfo/theforge
> >>theforge mail list group photo site is
> >>http://www.photoaccess.com
> >>Login:  [email protected]
> >>password:  anvil
> >>___________
> >
> >
> >_______________________________________________
> >http://mailman.qth.net/mailman/listinfo/theforge
> >theforge mail list group photo site is
> >http://www.photoaccess.com
> >Login:  [email protected]
> >password:  anvil
> >___________
> >
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________