I've also got one of the HF shears. Just came in from using it, in fact.
I've been using it on 16g with no problems at all. But it won't even
scratch 1/8".

-Marc

On Sat, 2003-01-18 at 16:51, Dave Brown wrote:
> At 16:24 01/18/03 -0500, you wrote:
> >Anyone have one of their throatless shears ? Any comments on it perhaps?
> >
> >Bob
> >HotAnvil Forge
> 
> Whose shears?  You didn't mention.  However, I have one of the HF 
> throatless shears and like it.  It's not designed for cutting 14ga, but 
> does just fine on 18 and lighter.  The HF throatless shear has done all 
> I've asked it to and the blades are still sharp.  My friend Jim Enloe has 
> one, but nicked the blades trying to cut some 1/8 stuff, but he still cuts 
> lighter stuff with it but has to avoid the nicks in the blades.
> 
> 
> Dave Brown
> Heritage Smithing
> Green Bay, WI
> ABANA, UMBA, GoM, MODA, ARG
> 
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
> 
> 

-- 
Marc Godbout
http://www.ironringforge.com