[TheForge] Sidearm Burner Parts - ceramic nozzle
Cameron Stoker
[email protected]
Thu Jan 16 12:39:00 2003
I've been curious about a castable ceramic product I've seen at
mcmastercarr.com. They have several grades available, here is the part
number for an alumina castable ceramic: 8498K35
They claim it is a room temp hardening dimensionally stable ceramic,
good to 3000 F. Sounds almost too good to be true, but maybe not at
$8.50 /lb. Still you could make a lot of burner flares with 10 pounds
of the stuff. Anyone have any experience with this (or similar stuff) ?
On Thursday, January 16, 2003, at 09:36 AM, terry l. ridder wrote:
>
> sidenote:
> at some point we really need to restart work on ceramic nozzles.
> a high alumina percentage refactory ceramic would be best.
> an alternate refactory would be silicon carbide.
>
Cameron Stoker
[email protected]
"May you run like a vicuna!"
pgp key @ http://keys.stoker.net