I've had several automatics, both cheap and expensive.
The cheaper units tend to take about 2X the time the best units do to
change.
The more expensive ones also tend to let more light thru the lens so you can
see your work piece in dim light conditions before you strike an arc.
If you are using the HF unit for extended welding sessions I recommend that
you
close your eye lids as you strike the arc, to insure you minimize the flash
burn.
Remember the arc damage is cumulative.