I did like you guys said. I coated my fork in vegi-oil, wiped it off and
threw it in the oven for half an hour at 400 deg. When I pulled it out it
had an amber colored film all over. I went ahead and steel-wolled it off
cause it was kind of tacky. Should I have left this on or did I do right?
It feels smooth now, I dont know, never done this before.