[TheForge] 1045 uses

Gladish Family [email protected]
Thu Feb 20 20:07:01 2003


I bet the guys on the woodworking list are sitting around right now talking
about that great piece of Bubinga that was almost a finished sculpture when
it split apart!
Iron- it's a living material, full of surprises...
Andy G

> I will also say that I
> have many times had the problem of a piece breaking off at an
> inopportune moment. with new steel as well as scrap.  Usually with new
> steel, it is because the piece given to me by the yard is higher carbon
> than what I specified.   Gee, this debate is beginning to shape up like
> another forge-weld vs arc/gas weld debate.
>