[TheForge] 1045 uses
Bob Bergman
[email protected]
Wed Feb 19 09:41:02 2003
Go find a truck shop and dig in their dumpster for leaf springs. These
are very easy to find around here.
----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Wednesday, February 19, 2003 7:46 AM
Subject: [TheForge] 1045 uses
> I want to make swages and special purpose tools for using under a 100
lb
> hammer. I have not had much luck finding "spring steel" which Clifton
Ralph
> recommended. I am wondering if there is a draw back to using 1045. I
know a
> lot of people use mild steel for swages but i am concerned that with
all the
> work that goes into these tools that the life span will be to short.
I have
> heard of carburizing mild steel but have no experience. I would like
to hear
> your recomendations.
>
> Ben
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>