[TheForge] Brushed finish
Chris Kilpatrick
[email protected]
Fri Feb 14 18:26:00 2003
passivation layers are layers of black oxide which can be acheived by dunking SS in a pot of boiling unsweetened kool-aid. That is how we passivated the primary loop on our reactors, then we ran a basic solution to cut down on rust. Stainless means it stains LESS not that it does not stain.
---
It is I who formed the blacksmith,
who fans the flame into a fire and
fashions a weapon fit for it's work.
On Thu, 13 Feb 2003 14:07:33
Bruce Freeman wrote:
>Because SS is not a uniform material. All SS that doesn't rust is passivated. Literally, the iron is etched out of the surface, leaving behind chromium and nickel. These form clear oxides - no rust. Cut through this outer layer and expose the iron and bingo, rust.
>
>Now wheter wire brushing WILL cut through this outer layer, I don't know. (A mild steel wire brush deposits mild steel on SS, so that's a different thing.) However, an abrasive pad certainly will cut through the outer layer, because the abrasives they put on those things are much harder than SS.
>
>Bruce
>NJ
>
>>>> [email protected] 02/13/03 01:24PM >>>
>Dan Scheid wrote:
>>
>> really, I thought that the property of stainless was in the material. Not in
>> the finish how fast will it rust ?
>> Dan Scheid
>>
>> > Don't forget that roughing the surface of stainless can make it subject to
>> > rusting. If it will be exposed to the elements, it will either need to be
>> > coated or pasivated.
>> > Darrell
>
>How does a rough finish change the inherent property of SS? I know that
>if you use a plain steel wire brush etc for the brushed look you can get
>some particles of steel in the SS that will rust,, but if you use a SS
>wire wheel you should not have this issue.
>
>
>Ralph
>
>
>
>
>
>"Good is the enemy of Excellent. Talent is not necessary for Excellence.
>Persistence is necessary for Excellence. And Persistence is a Decision."
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________
>
>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________
>
>
>
_____________________________________________________________
Get 25MB, POP3, Spam Filtering with LYCOS MAIL PLUS for $19.95/year.
http://login.mail.lycos.com/brandPage.shtml?pageId=plus&ref=lmtplus