[TheForge] Slack Tank
Rick & Kims Email
[email protected]
Wed Feb 5 20:03:02 2003
I have used stainless steel tubs: old swiming pool filter tanks or
1/2 barrels (the beer contailers). Cut off the top w/a plasma cutter.
No rust, no leaks.
Rick Korinek
Emerald City Forge
Framingham, MA
----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Wednesday, February 05, 2003 8:43 AM
Subject: Re: [TheForge] Slack Tank
> Yes, that's where I've gotten all of my 5 slack tubs (1 for each
county
> fair smithy we work at, our home smithy, and for the traveling
demo).
>
> The local going rate is about $25 for a half barrel and $45 for a
whole
> barrel. Our local garden center actually carries REAL whiskey
barrels
> from Seagrams. As long as they haven't been allowed to sit dry for
too
> long they will swell up and hold water pretty quick.
>
> As long as you don't let the water freeze in them (sometimes it
blows out
> the bottoms) they last a good long time.
>
> Dan Crowther
>
>
> > Rick lots of garden places sell the old whiskey barrels
for
> > planters......those might work.
> >
> > Ralph
> >
> >
>
>
> ---------------------------------------------
> This message was sent using Road Runner's Web-based
> e-mail.
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>