Bob, I think I am having a bad night.  Does you chuck have anything behind
the #34, as -02, or -33 or -06  if so then that is the taper size  -- a No.
2 or a No. 33 or a No. 6

Also if you need it the No. 6 is big end 0.676 small end 0.624 and length
1.000

Good night,

Dave Smucker
----- Original Message ----- 
From: <[email protected]>
To: <[email protected]>
Sent: Friday, August 29, 2003 8:10 PM
Subject: [TheForge] arbor size ?


> I have a jacobs #34 1/2  drill chuck does anyone have any idea what size
> jacobs taper it has so I can order the right size arbor
> Bob
> Hotanvil Forge
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
>   text/plain (text body -- kept)
>   text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment.  Attachments are not allowed.  To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html  ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>