[TheForge] arbor size ?
David E. Smucker
[email protected]
Fri Aug 29 22:41:00 2003
Bob,
I left one out -- it also my be a No. 33 (more likely than a No. 3) it
must be time to go to bed.
the dimensions of the tapers are as follows, big end 0.624
small end 0.561 and length of taper 1.000 again this is the male
Don't have anything to measure the female with -- try candle wax and then
check with a mic. Put a little vasoline in the hole before you pour candle
wax in place.
Dave Smucker
----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Friday, August 29, 2003 8:10 PM
Subject: [TheForge] arbor size ?
> I have a jacobs #34 1/2 drill chuck does anyone have any idea what size
> jacobs taper it has so I can order the right size arbor
> Bob
> Hotanvil Forge
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>