[TheForge] bar twisters

Ed F [email protected]
Wed Aug 27 07:50:01 2003


----- Original Message -----
From: "RIES NIEMI" <[email protected]>


> Ed- Dave's twister applies pressure thru the large spring which pushes the
> pipe clamp carriage away from the motor.

I was wondering how that gets accomplished.  Seems like you'd pull the
spring back and clamp it down after the bar is chucked up.  Dave, do you use
a come-along, hand force, ... etc?

Ed