[TheForge] Strengthening castable refractory
Steve Smith
[email protected]
Fri Aug 22 08:52:01 2003
I ran into some castable in Colorado that had fiber reinforcing in it.
Sorry but I don't have the manufacturer's name.
Steve Smith
Marc Godbout wrote:
> I'm building a new forge. This one will have an arched roof made out of
> insulating castable refractory. The insulation will be in a metal shell
> - a half-pipe. Is there anything I could, or even should, do to
> strengthen it? Chances are it will crack at some time in the future due
> to heat. Since it's arched, a crack straight through will probably not
> affect much. But multiple cracks at the wrong angle could let a chunk
> fall out.
>
> I have a roll of stainless steel wire. Would using this as a sort of
> "rebar" make a difference? Any other thoughts?
>
> Thanks.
>