[TheForge] Angled tenons

Ralph Sproul [email protected]
Tue Aug 19 08:28:01 2003


        Randy,  I've found a small drill press in the middle of a set of
stairs works for angle holes.
        I like your option of "split the bar and bend 1/2 ea. way and
rivet".   Thanks.

Ralph

----- Original Message -----
From: "R.C.Mundt" <[email protected]>
To: <[email protected]>
Sent: Monday, August 18, 2003 11:49 PM
Subject: Re: [TheForge] Angled tenons


> If the tennon is @ an angle then the hole it goes in must be @ an angle
also
> the whole thing is kinda a pain in the but.
> I made 1/2" round tennon"s on 1/2" square bar just tappered the bar w/ the
> grinder to start the monkey  tool then drove an angled  monkey tool on ,
it
> just rounded the corners. I arc welded the tennons in the hole and ground
> smooth, lookerd great just was not any fun, would much rather split the
bar
> and bend 1/2 ea. way and rivet.
> Randy Mundt
>
> ----- Original Message -----
> From: "Shannell Sugrue" <[email protected]>
> To: <[email protected]>
> Sent: Monday, August 18, 2003 8:52 AM
> Subject: Re: [TheForge] Angled tenons
>
>
> > Never done one but Ill state the obvious, that you can of course forge 2
> of
> > the sides under square dies in a PH by holding at the needed angle,
after
> > forging a normal tenon. That leaves the other 2 of which one of them,
the
> > long side could be done under off set dies but that still leaves a small
> > square sholder plus the other square sholder to, file/hack/grind to the
> same
> > angle you forged to. A lot less work than cutting the whole tenon
though.
> >
> > ----- Original Message -----
> > From: "Ralph Sproul" <[email protected]>
> > To: <[email protected]>
> > Sent: 18 August, 2003 8:39 PM
> > Subject: Re: [TheForge] Angled tenons
> >
> >
> > > Bob,  I've used a hack saw, as well as drilling and taping for a
> threaded
> > > insert then cut the shoulder angle to your needs for this previously,
> but
> > > I'm interested in others replies to this topic.
> > >
> > > Ralph
> > > ----- Original Message -----
> > > From: "Bob Smolen" <[email protected]>
> > > To: <[email protected]>
> > > Sent: Monday, August 18, 2003 2:02 AM
> > > Subject: [TheForge] Angled tenons
> > >
> > >
> > > > If a tenon meets the piece with the mortise at an angle other than
90
> > > deg.,
> > > > what is the method for putting this angle on the shoulders of the
> tenon.
> > > Is
> > > > it by the dreaded filing technique, angled monkey tool or ??
> > > > Thanks,
> > > > Bob
> > > >
> > > > _______________________________________________
> > > > http://mailman.qth.net/mailman/listinfo/theforge
> > > > theforge mail list group photo site is
> > > > http://www.photoaccess.com
> > > > Login:  [email protected]
> > > > password:  anvil
> > > > ___________
> > > >
> > > >
> > >
> > > _______________________________________________
> > > http://mailman.qth.net/mailman/listinfo/theforge
> > > theforge mail list group photo site is
> > > http://www.photoaccess.com
> > > Login:  [email protected]
> > > password:  anvil
> > > ___________
> > >
> > >
> > >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>