If the tennon is @ an angle then the hole it goes in must be @ an angle also
the whole thing is kinda a pain in the but.
I made 1/2" round tennon"s on 1/2" square bar just tappered the bar w/ the
grinder to start the monkey tool then drove an angled monkey tool on , it
just rounded the corners. I arc welded the tennons in the hole and ground
smooth, lookerd great just was not any fun, would much rather split the bar
and bend 1/2 ea. way and rivet.
Randy Mundt
----- Original Message -----
From: "Shannell Sugrue" <[email protected]>
To: <[email protected]>
Sent: Monday, August 18, 2003 8:52 AM
Subject: Re: [TheForge] Angled tenons
> Never done one but Ill state the obvious, that you can of course forge 2
of
> the sides under square dies in a PH by holding at the needed angle, after
> forging a normal tenon. That leaves the other 2 of which one of them, the
> long side could be done under off set dies but that still leaves a small
> square sholder plus the other square sholder to, file/hack/grind to the
same
> angle you forged to. A lot less work than cutting the whole tenon though.
>
> ----- Original Message -----
> From: "Ralph Sproul" <[email protected]>
> To: <[email protected]>
> Sent: 18 August, 2003 8:39 PM
> Subject: Re: [TheForge] Angled tenons
>
>
> > Bob, I've used a hack saw, as well as drilling and taping for a
threaded
> > insert then cut the shoulder angle to your needs for this previously,
but
> > I'm interested in others replies to this topic.
> >
> > Ralph
> > ----- Original Message -----
> > From: "Bob Smolen" <[email protected]>
> > To: <[email protected]>
> > Sent: Monday, August 18, 2003 2:02 AM
> > Subject: [TheForge] Angled tenons
> >
> >
> > > If a tenon meets the piece with the mortise at an angle other than 90
> > deg.,
> > > what is the method for putting this angle on the shoulders of the
tenon.
> > Is
> > > it by the dreaded filing technique, angled monkey tool or ??
> > > Thanks,
> > > Bob
> > >
> > > _______________________________________________
> > > http://mailman.qth.net/mailman/listinfo/theforge
> > > theforge mail list group photo site is
> > > http://www.photoaccess.com
> > > Login: [email protected]
> > > password: anvil
> > > ___________
> > >
> > >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>