I just had a thought (uh-oh)...
What if you were to add oxalic acid in some portion to the flux in order to
destroy the scale? Am I delusional, or could that potentially eliminat the
need for wire brushing and make welding odd shapes and angles easier? Input
is greatly appreciated before I try this and wind up killing myself :-)
happy hammering,
Carl Tappan

At 06:31 PM 8/16/2003 -0500, you wrote:
>At 10:55 08/15/03 -0700, you wrote:
>>All hands:
>>
>>     Although I have seen posts regarding the addition of flourspar (sp?) 
>> and boric acid powder to anhydrous borax for allegedly superior welds, 
>> none have mentioned the mixing proportions.  Does anyone out there have
these?
>>
>> 
>>Grant
>
>I've heard, but can't vouch for, boric acid added at anywhere from 20% to 
>30%.  Once tried the 25% level, but can't say if it was better or not.  Not 
>enough trying on my part.
>
>Dave Brown
>Heritage Smithing
>Green Bay, WI
>ABANA, UMBA, GoM, MODA, ARG
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________
>
>
>
>
>
Carl Tappan
(978) 263-7346
867 Liberty Square Rd.
Boxborough, MA 01719

http://www.bluetoadforge.com

"Gold for the mistress, silver for the maid. 
Copper for the craftsman, cunning in his trade."
"Well," said the baron, sitting in his hall. "But iron, cold iron is the
master of them all."