Thanks alot guys, good info as usual.
Bill Woolley
[email protected] wrote:
>Don't know if anyone mentioned it but you can use the shortcut of
>80 x dia. of hole in inches x thickness of metal in inches will equal
>the tonnage needed to punch the hole in mild steel. So like Dan
>said (I think his Whitney 20 is rated at 20 tons) Dan's example
>would be 80 x .5 x .5 = 20tons for half inch hole in half inch plate.
>
>With the variables involved you should probably figure on using a
>tonnage of at least 50 percent more.
>