[TheForge] Stick welding question

Paul Hewitt [email protected]
Fri Aug 8 02:01:00 2003


whats amusing is I live in 90% humidity environment, and my rods sit open
365 days a year and of those 365 days 50% of them are 100% humidity........
I never have a problem.  of course my box of rods never last more than 3 or
4 years  (50# at a time i buy them new).


----- Original Message -----
From: "Phil" <[email protected]>
To: <[email protected]>
Sent: Thursday, August 07, 2003 12:04 PM
Subject: Re: [TheForge] Stick welding question


> Ralph will probably disagree with me, he always does on arc welding
questions, but if the rods are really old, I'd get rid of them.  You could
try to dry out a few just for the heck of it.  You can get 6013s in 1 and 5
pound boxes I think, and just not keep so much on hand.
>
> > Thanks...I got a box (20 lbs) of free rods (6013) from a school metal
shop
> > that was closing.  The rod was really old and sitting in a cardboard box
in
> > a closet for years.  I am betting humidity unless flux can spoil???
I'll
> > try baking them for a bit
> >
> > Temperature?  time?  Can I just put them on a stainless steel broiler
> > pan?....Will it ruin the pan?
> >
> > Dan
> > -----Original Message-----
> > From: Ralph Sproul <[email protected]>
> > To: [email protected] <[email protected]>
> > Date: Thursday, August 07, 2003 12:32 PM
> > Subject: Re: [TheForge] Stick welding question
> >
> >
> > >Dan,  It sounds like if you have the same welder, on the same amperage,
> > >using the same rods,  it is a humidity problem with all the rain and
humid
> > >weather we've had lately.  If the flux is blistering off when you
strike
> > and
> > >arc that is definitly the problem - but that's usually when it's real
bad.
> > >
> > >Ralph
> > >----- Original Message -----
> > >From: "irontree" <[email protected]>
> > >To: <[email protected]>
> > >Sent: Thursday, August 07, 2003 10:15 AM
> > >Subject: [TheForge] Stick welding question
> > >
> > >
> > >> Hey all,
> > >>
> > >> I need some welding advice.
> > >>
> > >> I have an old Lincoln buzz box (220 volts, 50 amps).  Lately my welds
> > have
> > >> been filled with bubbles.   What's wrong?
> > >>
> > >> possiblilties:  Old sticks?, too much amperage?, sticks left sitting
out
> > >> (humidity)?, etc.
> > >>
> > >> Any advice?
> > >>
> > >> Dan
> > >> www.irontreeworks.com
> > >>
> > >>
> > >>
> > >> _______________________________________________
> > >> http://mailman.qth.net/mailman/listinfo/theforge
> > >> theforge mail list group photo site is
> > >> http://www.photoaccess.com
> > >> Login:  [email protected]
> > >> password:  anvil
> > >> ___________
> > >>
> > >>
> > >
> > >_______________________________________________
> > >http://mailman.qth.net/mailman/listinfo/theforge
> > >theforge mail list group photo site is
> > >http://www.photoaccess.com
> > >Login:  [email protected]
> > >password:  anvil
> > >___________
> > >
> > >
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>