[TheForge] More Finishing Stuff
Carl T
[email protected]
Tue Aug 5 18:16:01 2003
Hey all
I have been making a pile of kitchen forks lately, and am wondering if
there is a good treatment for them that will prevent rust when they are
washed, but not affect the taste of the food. Oil-Blackening is out, since
it leaves black crud on anything, as is rustoleum since it will flake off
when run through a dishwasher repeatedly. I am wondering about maybe
finishing it with beeswax, since I don't remember that as having much
taste, but could be confused. Any input would be greatly appreciated.
Thanks a Bunch.
Happy Hammering,
Carl Tappan
Carl Tappan
(978) 263-7346
867 Liberty Square Rd.
Boxborough, MA 01719
http://www.bluetoadforge.com
"Gold for the mistress, silver for the maid.
Copper for the craftsman, cunning in his trade."
"Well," said the baron, sitting in his hall. "But iron, cold iron is the
master of them all."