[TheForge] NEW - weld question

[email protected] [email protected]
Fri Apr 25 07:22:00 2003


A Weld-Pak 155 is a very capable machine. Be sure you have penetration, and if needed use successuve passes. A little preheat always helps.

Ray Miller
Cincinnati

> 
> From: "Mark Pesetsky" <[email protected]>
> Date: 2003/04/24 Thu PM 02:31:52 EDT
> To: <[email protected]>
> Subject: [TheForge] NEW - weld question
> 
> 
> 
> 
> I have a LINCOLD Weld-Pak 155 and I was wondering if I could weld some 1/4"
> "I" beam to a mild plate w/o a gas conversion using flux core welding wire.
> Is this something that could be done with a strong enogh weld for the air
> hammer that I am building?
> 
> The specs for the said welder are as follows:
> 
> 
> Welding Specifications
> Rated CV Output Amps/Volts/Duty Cycle Output Range Wire Feed Speed Range
> (IPM) Wire Feed Speed Range (M/MIN) Solid Wire Size Range Cored Wire Size
> Range
> 208V: 130/20/25%
> 230V: 130/20/30% 30-175A DC 50-400 1.3-10.2 .025-.035" .035-.045"
> 
> 
> Thanks In Advance
> Mark
> 
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
> 
> 
>