[TheForge] Swedge block question

Bob Rackers [email protected]
Tue Apr 22 08:22:00 2003


I appreciate the alternative solution. However, it doesn't answer the original
questions.
I have other considerations which made me decide to use 3/4" in the first
place.
I didn't go into them in order to keep the problem simple.
The exact half-round profile doesn't have to be exact, nor does the length.
I'm trying to see just how far I can go from the original size and still have
the strength I need for the job.
It's possible I may have to leave a certain length in the full round, and if
so, I don't know how much.
I also have to have full 3/4" at the other end.

And even if I were to go that route, which was one consideration, it still
would leave my original questions unanswered.
Suppose you had to get it done today, had no other stock, and couldn't get any
other stock quickly enough.
Given that situation, what's the most efficient way to do it?
Alternative solutions are obviously more than welcome, but I'm still wondering
if anyone has the answers to the questions.

Bob

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Phlip
Sent: Tuesday, April 22, 2003 12:46 AM
To: [email protected]
Subject: Re: [TheForge] Swedge block question



Dunno, but it seems to me that you're doing things the hard way. If it were
mine to do, I'd swage down some stock with a slightly over-sized cross
section into the shape I needed, get it into the planar alignment I wanted
with heat and a soft-faced heavy hammer, make my bends ( hard way bends are
perfectly easy with a starting crease and a bright orange heat),
flatten/straighten my curve with the same heavy, soft-faced hammer, then
forge weld the 3/4 inch round back on, with a simple lap joint....bending it
flat then, if needed.

But then, I believe in getting a job done in THIS lifetime....

Phlip

 If it walks like a duck, and quacks like a duck, it is probably not a
cat.

Never a horse that cain't be rode,
And never a rider who cain't be throwed....


_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________