[TheForge] Re: wooden wedges

George Dixon [email protected]
Fri Apr 18 09:48:04 2003


Wood wedges will keep scale from filling the anvil 'pit'.  The vibration 
of hammering can allow scale to work under the anvil installation which 
can (over time) build up under the anvil base and cause it to tilt.
G Dixon