[TheForge] Brand New Topic-Stainless Pans

Ian [email protected]
Mon Apr 7 23:04:00 2003


Hey Paul, SHUT UP!..................... hehehehe

----- Original Message -----
From: "Paul Hewitt" <[email protected]>
To: <[email protected]>
Sent: Monday, April 07, 2003 7:51 PM
Subject: Re: [TheForge] Brand New Topic-Stainless Pans


> Dang someone needs to tell me to just SHUT UP....
>
> I would recommend you find a small rollforming shop, I suspect there are
> probably a few in your area, that can roll form any size or shape of pan
you
> want, and from any material.
>
> Use AltaVista, or 1blink and they will pop up about 400 roll form shops
> nation wide, and in Canada.
>
> I have found in the past that the rollforming is pretty cost effective
when
> you don't ask for precision, and want to surface finish the part yourself.
>
> ----- Original Message -----
> From: "Stephen McGehee" <[email protected]>
> To: "The Forge" <[email protected]>
> Sent: Monday, April 07, 2003 7:21 PM
> Subject: [TheForge] Brand New Topic-Stainless Pans
>
>
> > I have a client who wants some pedestals made that will support a
> > serpentine slab of glass, 9 feet long.  The pedestals are composed of a
> > pan-like base(think omelet or gold mining pans in shape) an inverted
> > cone column, topped by another pan with a solid top.  the bottom pan is
> > 13 in. by 2-3/8", the top is 17-3/8" by 3-3/16", all stainless.
> >
> > My question is: anyone know of a stamping company that makes stock domes
> > for tank fabrication?  This is not the opportunity to make hand hammered
> > bowls, it is an opportunity to fab something to look pretty and hold up
> > a $ 400 piece of  3/4 inch glass.  Any other potential source would be
> > sincerely appreciated.
> >
> >
> >
> >  Stephen McGehee
> >  Publisher of
> >  Irony, the sketchbook of an apprentice blacksmith
> >  P. O. Box 9822  Pine Bluff, AR 71611
> >  [email protected]
> >  (870) 540-0142
> >  (479) 643-3299 (farm)
> >  You can see a sample of IRONY magazine here:
> >
> >   http://lametalsmiths.org/news/page4.htm  )
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>


---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.467 / Virus Database: 266 - Release Date: 4/1/2003