[TheForge] pitted anvil

Dan Tull [email protected]
Fri Apr 4 20:44:01 2003


$14/# here
dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message -----
From: "John Chobrda" <[email protected]>
To: <[email protected]>
Sent: Friday, April 04, 2003 6:33 PM
Subject: Re: [TheForge] pitted anvil


> Dan;
>     see if you can find a welder in your area who does hard faceing and
buy a
> couple of rods from him. I have used MG 750 to repair anvils, but at over
$9.00 a
> pound and only coming in ten pound boxes it's a little expensive to fix
only one
> divot.
> John C.
>
> [email protected] wrote:
>
> > Hey all,
> >        Two questions
> >
> > 1.  How do I fix a pit in my anvil.  I have one deep pit (about .25"
deep, .5 "
> > dia) I have a old Lincoln stick welder and oxy/acetylne....can I fix it?
> >
> > 2.  My wife suggests that I go get another anvil. (I love my
> > wife!!)....new...or at least new condition ...(tween 150 and 250 lbs)
> > suggestions????  what should I plan on spending?
> >
> > Dan
> > www.irontreeworks.com
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>
>