[TheForge] chinese ASOs

Gladish Family [email protected]
Tue Apr 1 00:20:02 2003


Yah, what he said.   ;0

> Actually, I don't think brass does anything in a quench ( other than 
> contract).   It is the heating that softens the brass, not the quench.  
> 
> Charles
> 
> Gladish Family wrote:
> 
> >If it has to go over critical to be brazed, why couldn't it be hardened
> >(Quenched) on the way down?
> >What would that do to the brazing? Brass softens in a quench, so 
> it wouldn't
> >get brittle or anything...
> >Andy
> >