How does one sandblast paint and not have the sand embed itself in the paint
layer?
Bob
-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Shannell Sugrue
Sent: Saturday, September 21, 2002 9:40 AM
To: [email protected]
Subject: Re: [TheForge] joining powder coated pieces
Thats what Im doing with railings this week, use a good zinc undercoat and
paint it to match. I just wire wheel off the powder.
heres a tip,
to get a matt powdercoat which is impossible using any powder available here
in Aussie, I get a double coating of black, its called matt but its very
glossy, then I give that a very light sandblast and they come up looking
nice and matt, means you can even paint the powder coat because the paint
has something to key into, I often do a dry brush technique over the black.