I'll try to get some pictures posted. My son is talking about getting a
digital camera after the Chicago knife show in two weeks.
I came up with a third option on the basket. After opening them I quenched
them in water. And wvien though they are mild steel they seem to have
hardened enough to support themselves. Kind of in a wait and see mode right
now.
Bob Ehrenberger
Shelbyville, Mo
Subject: Re: [TheForge] Basket conversion
Reply-To: [email protected]
Hi Bob!
On Mon, 02 Sep 2002, Bob Ehrenberger wrote:
> Hi guys,
> I just finished a set of candelabra for my daughter's wedding next month.
> They really came out nice except that I put an open basket in the middle
of
> the main upright, and didn't use heavy enough stock. I used 4 bars of 1/4"
> and they just don't have the strenght to to support the weight.
Pics?
--