[TheForge] grinding wheel question
[email protected]
[email protected]
Wed Oct 23 14:32:00 2002
80 Grit is by far the most popular grit for most industrial grinders. You
can spark-out and have a super polished surface finish of maybe 6-8 micro, or
just rough grind to a 20 micro. The 46 grit can be used for really ripping
off stock.