Yes, thats a very good moisture cured Urethane.  Its better brushed on, and
works good on rough surfaces like a casting.  I would want to verify its
resistance to UV though if its going outside.


----- Original Message -----
From: "T.L.Tallman" <[email protected]>
To: <[email protected]>
Sent: Thursday, October 17, 2002 7:23 AM
Subject: Re: [TheForge] Painting Cast Aluminum fountain for outdoors


> try .......por15.com .......drys like a rock works  better on rusty metal
> comes off of nothing when dry nails skin ect ect
> high $$$ but goes a long way i qt did both sides of a v.w. floor pan 2
coats
> for instance terry
> ----- Original Message -----
> From: "Ken Showalter" <[email protected]>
> To: <[email protected]>
> Sent: Wednesday, October 16, 2002 12:16 PM
> Subject: [TheForge] Painting Cast Aluminum fountain for outdoors
>
>
> > Just got a 3-tier aluminum fountain which will be installed as the Peace
> Fountain at my wife's school.
> > It comes unpainted and rough(from Mexico) and after I grind it smooth am
> going to paint it black.
> > My thought is to prime it with metal primer and use several coats of
epoxy
> paint. Any suggestions?
> > Thanks-Ken
> >
> >
> >
> >
> >
> > --- StripMime Report -- processed MIME parts ---
> > multipart/alternative
> >   text/plain (text body -- kept)
> >   text/html
> > The reason this message is shown is because the post was in HTML
> > or had an attachment. Attachments are not allowed.
> > Please post in Plain-Text only.---
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>