[TheForge] Hossfeld vs Diacro
Andrew Vida
[email protected]
Mon Oct 7 13:01:01 2002
The DiAcro is a finer machine in terms of manufacture. It is capable of =
greater accuracy, which in the case of most black smithing is probably =
overkill. I'm not an expert in the use of either, but the Hosssfeld =
*may* be a bit more versatile.
-----Original Message-----
From: John Chobrda [mailto:[email protected]]
Sent: Friday, October 04, 2002 8:02 PM
To: The forge
Subject: [TheForge] Hossfeld vs Diacro
For the type of work being done in today's shops, is there any advantage
of one of these benders over the other? I have seen a lot of postings
about acquiring a hossfeld and was just wondering if there was a clear
advantage of one over the other. I have used the diacro but not the
hossfeld.
Thanks in advance
John C.
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________