It is proof coil chain. The grade for chain fall chain is grade 80... D.O.T.
chain must be grade 70 and so forth.,
----- Original Message -----
From: "Mike Spencer" <[email protected]>
To: <[email protected]>
Sent: Monday, September 30, 2002 2:44 AM
Subject: [TheForge] Chain fall chain


>
> Is the chain used on chain falls made to different size standards than
> ordinary harware store chain?
>
> I have a (probably quite old) light-weight chain fall that I
> collected years ago and have never used.  I want to rig it to move
> tools that are just a tad too heavy to casually move around by hand --
> a 300# anvil, a swage block or stove pipe crimper.  But it has no
> chain.
>
> Both a pretty old piece of chain and the new stuff in the hardware
> store have links that are just a tad too long.  They appear to fit
> but after a few turns, the chain rides up out of the slots in the
> wheels.
>
> Anybody know about the standards for this stuff?  If I drive 75
> miles to the industrial park and cruise the lift and hoist joints, am
> I likely to find the right stuff?
>
> It's marked "Yale Screw Geared Block -- 1/2 ton".  Seems to be in
> perfect shape except for a small, non-load bearing part that I can
> easily make.
>
> - Mike
>
> ---
> Michael Spencer                  Nova Scotia, Canada
>
> [email protected]
> http://home.tallships.ca/mspencer/
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>